The company developed a high-temperature primer for Metro wheels and its preparation method. The high-temperature primer for Metro wheels is composed of epoxy modified silicone resin as bonding base material, anti-corrosion pigments and fillers, aluminum silver paste, additives, solvent A as paint components, low molecular weight modified polyamide resin, cashew nut oil phenol modified aromatic amine resin, 4-6 (Dimethylaminomethyl) triphenol, adhesion promoter (silane coupling agent), solvent B as curing agent components, and an appropriate amount of diluent during construction. The main purpose of the invention is to develop a high-temperature coating product for Metro wheels with high-efficiency corrosion prevention, excellent salt spray resistance, rapid drying, strong adhesion, good physical and mechanical properties, easy construction, good chemical resistance, high temperature resistance and other comprehensive properties.
The company developed a high-temperature primer for Metro wheels and its preparation method. The high-temperature primer for Metro wheels is composed of epoxy modified silicone resin as bonding base material, anti-corrosion pigments and fillers, aluminum silver paste, additives, solvent A as paint components, low molecular weight modified polyamide resin, cashew nut oil phenol modified aromatic amine resin, 4-6 (Dimethylaminomethyl) triphenol, adhesion promoter (silane coupling agent), solvent B as curing agent components, and an appropriate amount of diluent during construction. The main purpose of the invention is to develop a high-temperature coating product for Metro wheels with high-efficiency corrosion prevention, excellent salt spray resistance, rapid drying, strong adhesion, good physical and mechanical properties, easy construction, good chemical resistance, high temperature resistance and other comprehensive properties.